Evaluation and Comparison of Salivary Nickel Levels in Patients Undergoing Orthodontic Treatment with Conventional Niti Wires and Teflon-Coated Niti Wires

Authors

  • Dr. Manoj Annamalai E PG Student Department of Orthodontics Rajarajeswari Dental College and Hospital Bangalore.
  • Dr. Shashi Kumar H C Professor Department of Orthodontics Rajarajeswari Dental College and Hospital Bangalore.
  • Dr. Shwetha GS HOD & Professor Department of Orthodontics Rajarajeswari Dental College and Hospital, Bangalore.
  • Dr. Syed Basheer Ahmed PGStudentdepartment Of Orthodontics Rajarajeswari Dental College and Hospital Bangalore.

Keywords:

Nickel-Titanium, Teflon-Coated Niti, Salivary Nickel, Orthodontic Archwire, Metal Ion Release; Biocompatibility.

Abstract

Objective: To evaluate salivary nickel levels at different time intervals in patients treated with conventional nickel-titanium (NiTi) wires and Teflon-coated NiTi wires, and to compare ion release between the two wire types.

Materials and Methods: Twenty patients aged 18–30 years undergoing fixed orthodontic treatment were randomly allocated to two groups of 10 each. Group 1 received 0.014-inch conventional round NiTi wires, while Group 2 received 0.014-inch Teflon-coated round NiTi wires. Unstimulated saliva was collected 1 hour before appliance insertion (T0), and at 7 days (T1), 14 days (T2), and 30 days (T3). Nickel concentrations was measured using atomic absorption spectrometry with a graphite furnace. Between-group comparisons were performed using independent Student t tests; changes over time were evaluated using repeated-measures ANOVA with Bonferroni post hoc comparisons.

Results: Baseline nickel concentrations wes comparable between groups. Nickel concentrations increased after appliance insertion and peaked at 14 days in both groups (Group 1: 8.068 ± 1.282 µg/L; Group 2: 4.120 ± 0.767 µg/L). At 7, 14, and 30 days, Group 1 demonstrated significantly higher nickel concentrations than Group 2 (p<0.001 for all post-insertion between-group comparisons).

Conclusion: Both wire types were associated with a time-dependent increase in salivary nickel, with peak release at 14 days and a subsequent decline by 30 days. Teflon-coated NiTi wires consistently showed lower post-insertion ion concentrations, indicating a potential barrier effect of the coating against metal ion release.

Downloads

Published

2026-11-14

How to Cite

Dr. Manoj Annamalai E, Dr. Shashi Kumar H C, Dr. Shwetha GS, & Dr. Syed Basheer Ahmed. (2026). Evaluation and Comparison of Salivary Nickel Levels in Patients Undergoing Orthodontic Treatment with Conventional Niti Wires and Teflon-Coated Niti Wires. International Journal of Pharmacy Research & Technology (IJPRT), 16(2), 8080–8088. Retrieved from https://www.ijprt.org/index.php/pub/article/view/3596

Issue

Section

Research Article